Abstract

The present invention provides a method for manufacturing an aluminum electrode using a solution process and an aluminum electrode manufactured thereby. The manufacturing method includes the steps of: manufacturing an aluminum precursor solution for the solution processing using AlH3 as a basic material before forming aluminum; coating the aluminum precursor solution on a substrate through the solution process and drying the aluminum precursor solution; and forming a low work function aluminum electrode through a low-temperature baking process at the temperature of at most 150° C. The method for manufacturing the aluminum electrode according to the present invention improves a thermal defect of the electrode due to a high-temperature baking process, prevents excessive loss of raw materials, and can manufacture aluminum electrodes of various sizes with area ranging from small to large at relatively low costs and by a simple process under atmospheric pressure.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 14 · Forward citations: 0.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A method for manufacturing an aluminum electrode using a solution process, the method comprising: manufacturing a solution containing an aluminum precursor (Step A); coating a first substrate formed of one of an inorganic material and an organic material non-reactive with the solution containing an aluminum precursor, with the solution containing an aluminum precursor (Step B); heating a second substrate formed of one of an organic material and an inorganic material, where an aluminum thin film electrode is to be formed, at a temperature of 80 to 150° C. (Step C); and after Step C, heating a c

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

Non-Patent Literature (1)

  • Machine Translation of KR 10-2010-0111411.