US 10,040,261 B2#135778559 Most CitedActiveUnited States (USPTO)Utility

Polyethylene useful for producing film and molded articles in a process which uses solid state stretching

0Forward Citations (#135778559 Global)
0.0/yrCitation Velocity (#135778559 Global)
0.56Citation PageRank (#135778559 Global)
50Prior Art Cited
3Claims (1 Indep. · 2 Dep.)
0Drawings / Sheets

Abstract

Applicants have discovered that certain polyethylene (PE) homopolymers or copolymers of ethylene and C3 to C10 alpha-olefin monomers are more suitable for oriented processes than other polyethylene resins. In an aspect, the PE has a MFI of 0.3 g/10 min. to 5.0 g/10 min., a melting point of from 110° C. to 140° C., a density of from 0.912 g/cm3 to 0.965 g/cm3(%), a haze of 10% or less, a clarity of at least 90, and a gloss of at least 60. The polyethylene is heated and formed into an article, cooled, and then the article is stretch oriented. In an embodiment, the film, tape, the melt extruded, injection blow molded, injection stretch blow molded, cast, and thermoformed articles that can be produced with this polyethylene has a thickness of 0.1 mil to 100 mils. The polyethylene exhibits excellent elasticity, toughness, stretch and optical properties for such applications.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 50 · Forward citations: 0.

Claims (3 — 1 Independent, 2 Dependent)

  1. Claim 1Independent Claim

    A method of making an article, comprising the steps of: providing, a resin, the resin consisting of a metallocene-catalyzed polyethylene/hexene copolymer having a melt flow index of about 0.9 g/10 min, a density of from 0.925 g/cm 3 to 0.935 g/cm 3 , and a melting point of from 110° C. to 140° C., wherein the zero shear viscosity in Pa-sec is about 2.8E+05; heating said resin and using casting to form a cast article; allowing the formed article to cool to a solid state; reheating the formed article; and orienting the article uniaxially or biaxially, thereby forming an oriented article.

  2. Claim 2Depends on #1

    The method of claim 1 , wherein the article is uniaxially oriented by stretching said article in a machine direction to produce a uniaxially-oriented article.

  3. Claim 3Depends on #1

    The method of claim 1 , wherein the article is biax

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

References Cited — Backward Prior Art (50)

PatentTitleYearCitations
US 2,919,462 AMethod of and apparatus for making plastic containers196025
US 3,456,044 ABiaxial orientation1969342
US 3,555,604 ABiaxial orientation197183
US 3,594,864 AMold actuated parison stretching device19716
US 3,608,032 AMethod for making a flexible container portion197110
US 3,651,196 APreparation of oriented polymeric strapping197239
US 3,768,948 ABlow mold197348
US 3,843,286 ABlow molding apparatus197445
US 3,855,380 AMethod for manufacturing unitary, seamless, collapsible thermoplastic tubes197480
US 4,054,630 AHot pin parison injection molding technique197718
US 4,207,063 AApparatus for molding hollow objects of thermoplastic resins19809
US 4,357,296 AInjection blow molding process198261
US 4,385,089 AProcess for preparing biaxially oriented hollow shaped articles from thermoplastic materials1983130
US 4,432,719 AApparatus for forming a blown thermoplastic article198418
US 4,510,301 AFluorocarbon copolymer films198542
US 4,592,720 ADevice for reheating and blow molding parisons198617
US 4,760,116 AMonolayer polyethylene shrink film198864
US 5,066,222 AMethod and apparatus for heating and conveying plastic preforms prior to mold blowing operations199144
US 5,194,324 AHigh gloss label face stock199342
US 5,472,791 AHeat shrinkable co-extruded film and relevant preparation procedure199515
US 5,543,223 AMoisture barrier film199630
US 5,594,071 AEthylene copolymer composition199732
US 5,942,326 AShrink film with good ink adhesion199918
US 5,945,221 ABiaxial orientation of fluoropolymer films199919
US 6,228,505 B1Medium density polyethylene film having unidirectional tear200121
US 6,322,894 B1Matte surface film with improved cuttability200123
US 2001048988 A1Polyolefin bottles and method for making same—31
US 2003039834 A1Low friction fibers, methods for their preparation and articles made therefrom—18
US 2003132186 A1Blow molded plastic container with inclined mouth and method and apparatus for obtaining same—8
US 2003148121 A1Metallized film having a medium density polyethylene layer—2