Method of production of hot dip galvannealed steel sheet with excellent workability, powderability, and slidability
Abstract
The present invention provides a method of production of hot dip galvannealed steel sheet with excellent workability compared with the Sendzimir method or non-oxidizing furnace method and further with excellent powdering or slidability, that is, a method of production of hot dip galvannealed steel sheet with excellent workability, powdering, and slidability characterized by processing a slab containing, by mass %, C: 0.01 to 0.12%, Mn: 0.05 to 0.6%, Si: 0.002 to 0.1%, P: 0.05% or less, S: 0.03% or less, sol. Al: 0.005 to 0.1%, and N: 0.01% or less and having a balance of Fe and unavoidable impurities by hot rolling, pickling, cold rolling, then annealing at 650 to 900° C., cooling to 250 to 450° C., holding at said temperature range for 120 seconds or more, then cooling to room temperature, pickling, preplating Ni or Ni—Fe without intermediate temper rolling, heating by 5° C./sec or more down to 430 to 500° C., galvanizing in a galvanization bath, wiping, then heating by a rate of temperature rise of 20° C./sec or more up to 460 to 550° C., not providing any soaking time or holding for soaking for less than 5 seconds, then cooling by 3° C./sec or more, and final temper rolling by a
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 26 · Forward citations: 2.
Claims (1 — 1 Independent, 0 Dependent)
- Claim 1Independent Claim
A method of production of a hot dip galvannealed steel sheet with excellent powdering, slidability, and reduction in coil break, the hot dip galvannealed steel sheet having an amount of deterioration of elongation with respect to a cold rolled steel sheet of 2% or less, characterized by processing a slab containing, by mass %, C: 0.01 to 0.12%, Mn: 0.05 to 0.6%, Si: 0.002 to 0.1%, P: 0.05% or less, S: 0.03% or less, sol. Al: 0.005 to 0.1%, N: 0.01% or less, and having a balance of Fe and unavoidable impurities, by sequentially hot rolling, pickling, cold rolling, then annealing at 650 to 900°
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (2 of 2 total)
References Cited — Backward Prior Art (26)
Non-Patent Literature (4)
- Machine translation of JP 2001303228.
- Machine translation of JP 2005256089.
- Office Action dated Feb. 24, 2009 for Korean Application No. 10-2007-7024006.
- Office Communication issued on Feb. 10, 2010 by the Chinese Patent Office in corresponding Chinese Application No. 2007800119574.