Copper alloy casting and method of casting the same

0Forward Citations (#113353396 Global)
0.0/yrCitation Velocity (#113353396 Global)
0.56Citation PageRank (#113353396 Global)
47Prior Art Cited
1Claims (1 Indep. · 0 Dep.)
0Drawings / Sheets

Abstract

Copper alloy casting contains Cu: 58-72.5 mass %; Zr: 0.0008-0.045 mass %; P: 0.01-0.25 mass %; one or more elements selected from Pb: 0.01-4 mass %, Bi: 0.01-3 mass %, Se: 0.03-1 mass %, and Te: 0.05-1.2 mass %; and Zn: a remainder, wherein [Cu]−3[P]+0.5([Pb]+[Bi]+[Se]+[Te])=60-90, [P]/[Zr]=0.5-120, and 0.05[γ]+([Pb]+[Bi]+[Se]+[Te])=0.45-4 (the content of an element ‘a’ is denoted as [a] mass %; the content of γ phase is denoted as [γ]% by area ratio; and an element ‘a’ that is not contained is denoted as [a]=0). The total content of α phase and γ phase is 85% or more, γ phase content is 25% or less by area ratio, and mean grain size in the macrostructure during melt-solidification is 250 μm or less.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 47 · Forward citations: 0.

Claims (1 — 1 Independent, 0 Dependent)

  1. Claim 1Independent Claim

    A copper alloy casting containing: Cu: 58 to 72.5 mass %; Zr: 0.0008 to 0.045 mass %; P: 0.01 to 0.25 mass %; one or more elements selected from Pb: 0.01 to 4 mass %, Bi: 0.01 to 3 mass %, Se: 0.03 to 1 mass %, and Te: 0.05 to 1.2 mass %; and Zn: a remainder, wherein the copper alloy casting satisfies the following equations, f1=[Cu]−3[P]+0.5([Pb]+[Bi]+[Se]+[Te])=60 to 90, f2=[P]/[Zr]=0.5 to 120, and f3=0.05[γ]+([Pb]+[Bi]+[Se]+[Te])=0.45 to 4, wherein the content of each element ‘a’ is denoted as [a] mass %, the content of γ phase is denoted as [γ]% by area ratio, and each element ‘a’ that is

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

References Cited — Backward Prior Art (47)

PatentTitleYearCitations
US 2,521,663 AElectron target and means for making the same195014
US 3,676,083 AMolybdenum base alloys197216
US 3,912,552 AOxidation resistant dispersion strengthened alloy197515
US 3,928,028 AGrain refinement of copper alloys by phosphide inoculation197527
JP S52107227 AHeat resisting cu alloy with excellent electro- and heat conductivity—11
US 4,110,132 AImproved copper base alloys197841
JP S5492516 ACu alloy for manufacture of seamless pipe—14
JP S5570494 AWire rod for copper welding excelling in electric conductivity, thermal conductivity and welding performance—24
US 4,238,249 AProcess for the preparation of a copper-zinc material198018
US 4,353,415 AHeat pipes and thermal siphons198240
JP S5839900 B2継目無し管製造用Cu合金—3
JP S61542 ACopper alloy for radiator plate—17
JP S61133357 ACu base alloy for bearing superior in workability and seizure resistance—35
JP S62274036 ACopper alloy having superior wear and corrosion resistance—26
JP S62297429 ACopper alloy having excellent corrosion resistance—20
US 4,822,560 ACopper alloy and method of manufacturing the same198969
JP H01162737 ACopper alloy for electronic parts—21
JP H03291344 ACopper alloy for heat exchanger header plate—12
JP H0658688 AInner surface grooved weld copper alloy pipe—12
WO 9,410,352 A1Pitting-resistant copper alloy pipe for water and hot-water supply—8
JP H06184669 APitting corrosion resistant copper alloy piping for feeding water and hot water—12
JP H06184674 AHigh electric conductivity copper alloy—5
US 5,370,840 ACopper alloy having high strength and high electrical conductivity199434
JP H111736 ABrass alloy material for heating device—28
US 5,871,861 ALithium ion secondary cell1999120
JP H1158034 AJoining method of ferrous material and high tension brass alloy and composite material joined by the method—24
JP 2000119775 ALead-free free cutting copper alloy—76
JP 2000199023 AElectric resistance welded copper alloy tube for heat exchanger excellent in 0.2% proof stress and fatigue strength—15
JP 2001247923 APitting corrosion resistant copper base alloy pipe material—24

Non-Patent Literature (5)

  • “Casting and Solidification Process,” dated Jan. 9, 2010, at http://classes.engr.oregonstate.edu/mime/winter2010/ie337-001/Laboratories/5.Solidification%20Lab.pdf, downloaded Nov. 23, 2011, three pages, filed in a related application as Exhibit B1.
  • “Exhibit A” (Metals Handbook Ninth Edition, vol. 9 Metallography and Microstructures, American Society for Metals, pp. 629-631).
  • “Exhibit C” p. E 41 of Glossary for Metalurgical Terms, The Japan Institute of Metals, 1995.
  • “Exhibit D” (ASM Metals Handbook 8th edition, vol. 8, Metallography, Structures and Phase Diagrams, 301 & D-2, American Society for Metals).
  • “Exhibit D” as filed in a corresponding related application (Binary Alloy Phase Diagrams, vol. 1, American Society for Metals, pp. 819-820, 971, 982 and 19).