Method for producing a nitrogen-alloyed steel by powder metallurgy
Abstract
In this method, a gas-atomized, spherical steel powder is charged in a capsule. The capsule and its contents are heated to a temperature of between 700 and 1000 degree C. Nitrogen gas with an absolute pressure of 0.1-1.5 bar is introduced into the capsule at the said temperature. The introduction of nitrogen gas continues at the rate at which the nitrogen is absorbed by the steel powder by diffusion into the steel and by being combined with nitride formers in the steel until a certain predetermined amount of nitrogen has been taken up in the steel. The introduction of nitrogen is then discontinued and the capsule is hermetically sealed. The temperature of the capsule and of its contents is increased to between 1050 and 1100 degree C and the steel undergoes a homogenizing treatment at a temperature of between 1050 and 1100 degree C, the nitrogen content gradients being essentially eliminated within the steel. The capsule is then subjected to hot isostat pressing to obtain complete sealing of the powder body. <IMAGE>
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 0 · Forward citations: 3.
Claims (0)
No claim text indexed for this record.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (3 of 3 total)
References Cited — Backward Prior Art (0)
No backward patent references recorded.