Forfarande for behandling av ett pyrithaltigt metalliskt ramaterial
Abstract
The method provides for the heating of the said raw material in a reducing atmosphere at a temperature of 450 to 500`C during 30 to 60 minutes. Hydrogen or products of conversion of the natural gas or of fuel-oil may be used as reducing atmosphere. The thus burnt copper-containing product is then cooled at a rate of 2 to 4 degrees per minute and subjected to a magnetic separation. The magnetic separation is carried out in two stages, ferrous sulphides being first extracted under a magnetic field intensity of 1000 to 2000 oersteds and then copper sulphides are extracted under a magnetic field intensity of 4500 to 6000 oersteds.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 0 · Forward citations: 0.
Claims (0)
No claim text indexed for this record.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (0 of 0 total)
No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.
References Cited — Backward Prior Art (0)
No backward patent references recorded.