Abstract
FIELD: chemical technology. SUBSTANCE: invention relates to substance emitting radiation in short-wave IR-spectrum and anions and to method for preparing this substance. For preparing such substance with emission in short-wave IR-spectrum the following substances are added to capacity, weight p. p.: silicon oxide, 50-55; potassium oxide, 2-4; aluminum oxide, 3-7; borax, 15-25; sodium oxide, 10-20, and calcium oxide, 3-7 followed by their mixing for 30-60 min. Mixture is placed into melting furnace at temperature 1200-1400 C and calcined for 1-3 h. Calcined material is cooled abruptly and ground. Phosphate rock in the amount 1-5 weight p. p. is added to the ground material and material is ground. Prepared substance shows high emitting capacity in short-wave IR-spectrum and emits simultaneously great number of anions designated for effect on human body. EFFECT: improved preparing method. 2 cl, 1 tbl
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 6 · Forward citations: 1.
Claims (0)
No claim text indexed for this record.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (1 of 1 total)
| Patent | Title | Year | Citations |
|---|---|---|---|
| RU 2,295,978 C2 | Method for carrying out thermal sterilization of infected waste materials | 2007 | 0 |