RU 2,201,636 C2#55108323 Most CitedExpiredInternational OfficeUtility

Phosphor mixture for coating glass bulbs of optical radiation sources

1Forward Citations (#55108323 Global)
0.0/yrCitation Velocity (#56453757 Global)
0.81Citation PageRank (#55108323 Global)
6Prior Art Cited
0Structured Claims
0Drawings / Sheets

Abstract

FIELD: electrical engineering; lighting lamp manufacture. SUBSTANCE: proportion of phosphor mixture ingredients is as follows, mass percent: powdered phosphor, 65.0-84.5; binder (boron oxide), 1.0-4.0; filler, the rest. At least 60% of powdered phosphor should have grain size up to 20 mcm. Quartz powder, milled sapphire powder, or crushed polycrystalline aluminum oxide may be used as filler. Ingredients are mixed up for 15-20 minutes, dried out at 100±5 C for 2.5-3.5 h, and cooled down. EFFECT: reduced cost of lamp manufacture; enhanced productivity of coating process. 1 tbl, 1 ex

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 6 · Forward citations: 1.

Claims (0)

No claim text indexed for this record.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (1 of 1 total)