Method for producing constructional powder steel
Abstract
FIELD: powder metallurgy. SUBSTANCE: method involves preparing powder mixture containing components of steel and bismuth powder added in an amount of 0.1-1.8% by weight; performing static cold pressing of powder mixture in closed mold to produce briquette with residual porosity of 20-30%; heating briquette in shielding atmosphere to temperature of 1.000-1.100 C; holding briquette at such temperature for 6-20 min; providing hot pressing by upsetting in closed mold to produce pore-free ready material, with value of specific power consumed for compression process being equal to 200-220 K/J/cub m. EFFECT: increased efficiency, simplified method, improved physical and mechanical properties of steel and high cutting processibility. 4 tbl
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 0 · Forward citations: 5.
Claims (0)
No claim text indexed for this record.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (5 of 5 total)
References Cited — Backward Prior Art (0)
No backward patent references recorded.
Non-Patent Literature (1)
- 1. Дорофеев Ю.Г. Порошковая металлургия. 1990, N6, с.9. 2. Иваненко Ф.А. Исследование и разработка технологии сварки металлокерамических малоуглеродистых материалов, полученных ДГП. В сб.: Исследование в области порошковой и стружковой металлургии. Т. 265. - Новочеркасск: НПИ, 1972.