Metallic build-up welding material of high tenacity and hardness and process for preparing the same
Abstract
The invention relates to a metallic material employed for build-up welding and to a process for preparing the same, the claimed material exhibiting good machining behaviour and high mechanical resistance under heavy erosion-abrasion impact wearing conditions combined with mechanical fatigue specific to surfaces which are in contact with natural aggregates, such as gravel, sand or ballast and crushed stone, upon breaking-grinding processes. According to the invention, the material consists, in mass percentage, of 4.60...6.80% Al, 20...22.50% Cr, 23...24.50% Fe, 23...24.50% Mn and 24...26.50% Ni, having a purity degree > 99%, a density in the range of 7.4...7.6 kg/dm, the liquidus temperature in the range of 1350...1400°C, an associated hardness of 700...950 HVafter specific heat treatments, a tenacity expressed as values of shock breaking energy of 55...70 J at a temperature of 20°C. The process, as claimed by the invention, consists in melting, in an induction furnace, the above-mentioned elements which are introduced in the following order: ARMCO-type Fe, Ni, Cr, Mn and, at the end of the smelting stage, Al, where, for substantially diminishing oxidation losses, the metal bath
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 0 · Forward citations: 0.
Claims (0)
No claim text indexed for this record.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (0 of 0 total)
No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.
References Cited — Backward Prior Art (0)
No backward patent references recorded.