Process for serpentinite processing, products and plant for making the same
Abstract
The invention relates to a process for serpentinite processing and to a plant for carrying out the process. According to the invention, the process consists of a first stage of solubilizing the serpentinite having a grain size of 63 μm, at the most, in an aqueous medium, at a temperature of 95...105°C and an atmospheric pressure, with recycling of acid process water, in the presence of nitric acid or hydrochloric acid 3...6 M solutions, in a second stage the said suspension being diluted and filtered, with separation of a liquid concentrated phase with Mg, Fe and Al content from a solid cake which, in the third stage is subjected to two washing cycles, after which, in the fourth stage, it is dried to result in a powder having a minimal content of 60% silicon dioxide, Si, Fe, Mg, while the acid solution resulting from filtration is treated with sodium nitrite and saturated alkaline sodium carbonate solution wherefrom an oxidic trivalent iron compound is precipitated, the filtrate resulting from the iron separation from the solution being then separated by precipitation with sodium hydroxide solution and saturated sodium carbonate solution until reaching a pH value of 11...12, wheref
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 0 · Forward citations: 1.
Claims (0)
No claim text indexed for this record.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (1 of 1 total)
| Patent | Title | Year | Citations |
|---|---|---|---|
| WO 2023/149792 A1 | Method for treating silicate and aluminosilicate rocks | — | 0 |
References Cited — Backward Prior Art (0)
No backward patent references recorded.