Sodium silicate production process
Abstract
The process comprises reaction of silica with NaOH. To increase performance, 40-45% NaOH, and siliceous powder waste (SiO2 content 91-95%) from ferrosilicon prodn. gas drying and cleaning, are dissolved and continuously stirring in water for 2.5-3 hours at 90-99 deg. C. The raw soln. is settled, filtered or centrifuged, to 1.36-1.70 g/cm3 and SiO2 28.08, Na2O 10.80, Fe2O3 0.040-0.095, CaO 0.020-0.036, and CaCl 0.08-0.20 wt.% contents.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 0 · Forward citations: 0.
Claims (0)
No claim text indexed for this record.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (0 of 0 total)
No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.
References Cited — Backward Prior Art (0)
No backward patent references recorded.