Electrods production method for water activated batterys
Abstract
The process comprises heat treatment at 80-125 deg.C of CuCl2.2H2O with or without AgCl or PbCl2 treated at 100-150 deg.C for 4 hrs. and with temp. rise of 0.4-0.125 and 0.4-0.1 deg.C/min. respectively. Pouring into closed moulds for pressing, and coating of the prod. with a thin film by dipping in AgCl-AgI or PbCl2 at 500 deg.C, facilitates the use of anodes of Al, Zr, etc. The discharge characteristics are superior to those of Cu2Cl2 electrodes and the activation time is less than 60 seconds. The mass capacity is 180 Ah/g.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 0 · Forward citations: 0.
Claims (0)
No claim text indexed for this record.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (0 of 0 total)
No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.
References Cited — Backward Prior Art (0)
No backward patent references recorded.