Abstract
To manufacture the implant a nanopowder of synthetic hydroxyapatite (HAp) is used having a hexagonal structure, average grain size in a range from 3 to 30 nm and the specific surface area greater than 200 m2 /g. First the nanopowder is formed to the desired geometric shape, and then the shape is fixed. In the step of shape formation the dried nanopowder is pressed in the mold under the pressure ranging from 50 MPa to 2 GPa. In the step of fixing the pressed nanopowder at room temperature is subjected to the pressure rising from the ambient value to the peak value selected from a range of 1 to 8 GPa and to a temperature selected from a range of 100º C to 600º C for a period of time selected from a range from 30 seconds to 5 minutes. The density of thus produced implant, determined by helium method, is not less than 75% of the theoretical density. The average grain size of the material forming the implant, determined according to the PN-EN standard, is not larger than 50 nm. The nanohardness of this material, measured using a Berkovich indenter and the load of 4 m N, is not less than 3 GPa, while the solubility, determined according to ISO 10993-4, is from 5 to 35 mg/dm3.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 0 · Forward citations: 1.
Claims (0)
No claim text indexed for this record.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (1 of 1 total)
| Patent | Title | Year | Citations |
|---|---|---|---|
| US 2022354651 A1 | Bone implant having coated porous structure | — | 0 |
References Cited — Backward Prior Art (0)
No backward patent references recorded.