Patents
PL 162,541 B1#127190377 Most CitedExpiredInternational OfficeUtility

Method of obtaining copper (ii) oxide

0Forward Citations (#127190377 Global)
0.0/yrCitation Velocity (#127190377 Global)
0.56Citation PageRank (#127190377 Global)
0Prior Art Cited
0Structured Claims
0Drawings / Sheets

Abstract

Manner of obtaining copper oxide /II/ through the oxidation of copper charges, characterized by the fact that the copper charge is initially oxidized in the temperature of 500-850 degrees Celsius and, then, the product of oxidation is quickly cooled by means of inserting into water and following this the excess water is separated by way of decantation and filtering off and the wet roasted ore is ground to the granulation of 0.3-0.6 and immediately following the grinding the wet slurry is further oxidized in the temperature of 500-750 degrees Celsius.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 0 · Forward citations: 0.

Claims (0)

No claim text indexed for this record.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

References Cited — Backward Prior Art (0)

No backward patent references recorded.