FremgangsmÕte for fremstilling, fortrinnsvis fra avfallsmaterialer, av silikatskum med lukkede porer, og produktet produsert ved fremgangsmÕten
Abstract
The process of the invention characterized in that to 100 parts by weight of a silicate powder having 2000-8000 m2/g specific surface, 1-10 parts by weight of gas-forming material with particle size of 10-100 mum and 0.5-15 parts by weight of montmorillonite, 0.5-2 parts by weight of alkali hydrogen phosphate or alkali dihydrogen phosphate or a mixture of alkali metal phosphate and sodium silicate in form of aqueous solution, 0.01-5 parts by weight of rare earth metal oxide or a mixture of such oxides were added, then the mixture obtained is homogenized, pre-dried, coated with 1-5 parts by weight of titanium oxide and/or titanium oxide hydroxide and/or aluminum oxide hydroxide, then subjected to heat treatment at 720-1000° C., and the mixture obtained is molded. The subject of the invention: also the product of the above process.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 0 · Forward citations: 0.
Claims (0)
No claim text indexed for this record.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (0 of 0 total)
No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.
References Cited — Backward Prior Art (0)
No backward patent references recorded.