Method for heat-treatment of a bonding wire for semiconductor device
Abstract
[ISSUES TO BE SOLVED] TO ACQUIRE THE BEST COMBINATION OF ELONGATION AND BREAK STRENGTH ON THE AU ALLOY BONDING WIRE. [SOLUTION MEANS] ADDING 0.5-30 MASS % OF AT LEAST ONE ELEMENT AMONG CU, AG, PD AND PT TO HIGH PURITY AU, A FLAT AREA ABOUT ELONGATION RATIO CHANGE APPEARS BETWEEN THE RANGE OF 450-650 ºC OF HEAT-TREATMENT TEMPERATURE AT WIRE DRAWING. THOUGH THE WIRE STRENGTH BECOMES DECREASE AT THIS RANGE OF TEMPERATURE, THE STRENGTH IS MAINTAINED AT HIGHER LEVEL AGAINST THE HEAT TREATMENT TEMPERATURE OF A STANDARD ELONGATION RATIO OF 4 % OF HIGH PURITY AU ALLOY WIRE. THEREFORE, BY THE HEAT TREATMENT OF THIS FLAT RANGE, AU ALLOY BONDING WIRE, WHICH HAS CERTAIN LEVEL OF STRENGTH REGARDLESS OF THE TEMPERATURE CHANGE, IS ACQUIRED. MOREOVER, BY SELECTING APPROPRIATE TEMPERATURE RANGE, DIFFERENT STRENGTH CHARACTERISTICS WIRES CORRESPONDING TO THE ELONGATION RATIO ARE ACQUIRED.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 0 · Forward citations: 0.
Claims (0)
No claim text indexed for this record.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (0 of 0 total)
No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.
References Cited — Backward Prior Art (0)
No backward patent references recorded.