Process of leaching a lateritic ore for preparing metal extraction
Abstract
THE STARTING MATERIAL IS LATERITIC ORE HIGH CONTAINS NICKEL OXIDE AND/OR COBALT OXIDE. FROM WATER AND COMMINUTED ORE, OF WHICH AT LEAST 80-WTHAVE GRAIN SIZES OF NOT MORE THAN 0.5 NM, A PUMPABLE SUSPENSION IS FORMED. THE ORE-CONTAINING SUSPENSION IS PASSED THROUGH AN INDIRECTLY HEATED PREHEATING TUBE, THE SUSPENSION BEING HEATED TO 150 TO 250?C. THE HEATED PREHEATING TUBE, THE SUSPENSION IS PASSED THROUGH A MIXING LINE IN WHICH AN ACID IN A MINIMUM AMOUNT OF 10KG PER 100KG ORE, CALCULATED ANHYDROUS, IS ADMIXED TO THE SUSPENSION AND THE ACID-CONTAINING SUSPENSION IS PASSED THROUGH AD WELL TIME TUBE IN WHICH THE DWELL TIME OF THE SUSPENSION IS AT LEAST 0.1 MINUTES. PREFERABLY, SULFURIC ACID IS INTRODUCED INTO THE MIXING LIUNE.@@FIGURE 1
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 0 · Forward citations: 0.
Claims (0)
No claim text indexed for this record.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (0 of 0 total)
No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.
References Cited — Backward Prior Art (0)
No backward patent references recorded.