Patents
MD 1740 Y#86017218 Most CitedActiveInternational OfficeUtility

Method for producing epitaxial TiO2 thin layers

0Forward Citations (#86017218 Global)
0.0/yrCitation Velocity (#86017218 Global)
0.56Citation PageRank (#86017218 Global)
0Prior Art Cited
0Structured Claims
0Drawings / Sheets

Abstract

The invention relates to the semiconductor manufacturing technology, and can be used for manufacturing optoelectronic devices.The method for producing epitaxial TiO2 thin layers comprises degreasing a glass substrate in toluene, drying it in isopropyl alcohol vapors and placing it in a chemical vapor deposition reactor, which is purged with argon for 20 min at a flow rate of 100 cm3/min, after which the temperature of the substrate is increased up to 400°C. The method also includes the formation of titanium isopropoxide vapors by bubbling at a temperature of 90°C. The deposition of epitaxial TiO2 layers is carried out by separately feeding into the reactor titanium isopropoxide vapors, carried by an argon flow at a speed of 40 cm3/min, and an oxygen flow at a speed of 40 cm3/min, for 30 min.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 0 · Forward citations: 0.

Claims (0)

No claim text indexed for this record.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (0 of 0 total)

No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.

References Cited — Backward Prior Art (0)

No backward patent references recorded.