A method for making a radial bearing
Abstract
In the process described, metal powder is mixed with not more than approximately 20 wt.% of ceramic particles, and the mixture is pressed to obtain a bearing of appropriate shape, while retaining a pore volume of at least 15 %. The pressed part is then sintered. The bearing hole is gauged to the final dimension uniquely by passing a gauging mandrel through the hole.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 1 · Forward citations: 0.
Claims (0)
No claim text indexed for this record.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (0 of 0 total)
No indexed citing patents in this generation yet. Ingest USPTO/PatentsView bulk citation tables via patents-ingest to expand the local forward citation graph.
References Cited — Backward Prior Art (1)
| Patent | Title | Year | Citations |
|---|---|---|---|
| US 3,137,927 A | Dispersion hardened materials | 1964 | 7 |