Patents
JP S6137418 A#37418151 Most CitedExpiredJapan (JPO)Utility

Thermoplastic polyetherether ketone film with lubricity

2Forward Citations (#37418151 Global)
0.1/yrCitation Velocity (#53720972 Global)
1.11Citation PageRank (#36298658 Global)
2Prior Art Cited
0Structured Claims
0Drawings / Sheets

Abstract

PURPOSE:To make it possible to obtain a thermoplastic polyetherether ketone film good in lubricity, by mixing 100pts.wt. thermoplastic polyetherether ketone with 0.01-10pts.wt. inorganic filler, and making the resulting composition into a biaxially oriented film. CONSTITUTION:A thermoplastic polyetherether ketone resin composition that is prepared by blending 100pts. wt. thermoplastic polyetherether ketone with 0.01- 10pts.wt. inorganic filler is made into a biaxially oriented film with lubricity and substantially made of the thermoplastic polyetherether ketone. The amount of the inorganic filler in the resin composition should be 0.01-10pts.wt., preferably 0.02-5pts.wt. to 100pts.wt. thermoplastic polyetherether ketone, and if the amount is less than 0.01pt.wt. the lubricity is unsatisfactory and if the amount exceeds 10pts.wt. the transparency decreases. The method of adding the inorganic filler may be the dry blending process, or other process using mixing machines such as a mixer, extruder, etc.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 2 · Forward citations: 2.

Claims (0)

No claim text indexed for this record.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (2 of 2 total)