High hardness sintered body and its manufacture
Abstract
PURPOSE:To manufacture a high hardness sintered body having superior wear resistance by mixing fine particles of cubic boron nitride or high pressure phase boron nitride with at least one among the carbide, nitride or carbonitride of Ti or Ti-Ta and Al and by sintering the mixture at high temp. and pressure. CONSTITUTION:Boron is added to a mixture consisting of 65-95vol% cubic boron nitride (CBN) or high pressure phase boron nitride consisting of 70-95vol% CBN and 5-30vol% wurtzite type boron nitride (WCN), 4-34vol% at least one among the carbide, nitride and carbonitride of Ti or Ti-Ta and the balance Al. The boron nitride is used in the form of particles having 10-50mum maximum particle size and <1mum minimum particle size, and the amount of the boron added is 0.1-5vol% of the amount of the mixture. They are mixed and sintered at 1,200 deg.C minimum temp. under 20,000 atm. minimum pressure to manufacture a high hardness sintered body having high wear resistance. In the sintered body, the mixed hard starting materials are firmly bonded to each other with TiB2 and AlN formed during the sintering.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 7 · Forward citations: 6.
Claims (0)
No claim text indexed for this record.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗