Chemical vapor deposition method
Abstract
PURPOSE:To form efficiently a dense vapor-deposited layer with high hardness by introducing a reactive gas consisting of H2, WF6 and N2 in a specified ratio into a reaction chamber contg. a material to be plated and by heating the material to carry out chemical vapor deposition. CONSTITUTION:A material 3 to be subjected to vapor deposition is mounted on a table 4 in a tubular reaction chamber 1 provided with a heating furnace 2 around the chamber 1. H2, N2 and WF6 are fed from cylinders 5, 6, 7 and introduced into the chamber 1 from the inflow hole 1a as a gaseous mixture, and the material 3 is heated to 400-700 deg.C to carry out vapor deposition. The molar ratio of WF6:H2 in the gaseous mixture is (1:3)-(1:1), and the molar ratio of N2 to WF6+H2 is 0.05-5.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 0 · Forward citations: 7.
Claims (0)
No claim text indexed for this record.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (7 of 7 total)
References Cited — Backward Prior Art (0)
No backward patent references recorded.