Preparation of lead core
Abstract
PURPOSE:To obtain a lead core having a high concentration and smooth feeling in writing with retained practical strength, by kneading a colorant and a binder with dinitronaphthalene, exrusion molding the resultant mixture, and calcining the molded material at a high temperature. CONSTITUTION:A colorant, e.g. graphite or carbon black, and a binder, e.g. polyvinyl chloride or 3,5-dimethylphenol-formaldehyde resin, are kneaded with preferably 0.5-30%, more preferably 1-20%, based on the binder, dinitronaphthalene, and the resultant mixture is then extrusion molded and calcined at a high temperaure of preferably 600 deg.C or above to give the aimed lead core. USE:Suitable for an extra lead for propelling pencil of 0.2-0.9mm. diameter.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 0 · Forward citations: 1.
Claims (0)
No claim text indexed for this record.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (1 of 1 total)
| Patent | Title | Year | Citations |
|---|---|---|---|
| US 5,733,482 A | Baked color pencil lead manufactured by impregnation with perhydropolysilazane and heat treatment | 1998 | 4 |
References Cited — Backward Prior Art (0)