Manufacture of high-tensile cold-rolled steel plate with heat hardenability for deep drawing
Abstract
PURPOSE:To obtain a cold rolled steel plate with superior deep drawability and heat hardenability by batchwise annealing a cold rolled steel plate contg. a specified percentage of C, Si, Mn, P, S, sol. Al and N at a specified temp. CONSTITUTION:Steel consisting of 0.002-0.025% C, <=0.20% Si, 0.25-1.00% Mn, 0.020-0.150% P, <=0.030% S, 0.020-0.120% sol. Al, 0.0050-0.160% N and the balance Fe with inevitable impurities is formed into a slab by ingot making or continuous casting. The slab is heated by an ordinary heating method while adjusting the finish outlet temp. close to the Ar3 transformation point or above. The heated slab is coiled at <= about 680 deg.C, cold rolled and annealed at the recrystallization temp. -760 deg.C for about 5-24hr in a batchwise annealing furnace. Refining is then carried out to obtain a high-tensile cold-rolled steel plate with heat hardenability for deep drawing.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 4 · Forward citations: 5.
Claims (0)
No claim text indexed for this record.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗