Manufacture of nonrefined high tensile steel

12Forward Citations (#8252615 Global)
0.3/yrCitation Velocity (#27296101 Global)
2.65Citation PageRank (#9231298 Global)
0Prior Art Cited
0Structured Claims
0Drawings / Sheets

Abstract

PURPOSE: To manufacture a nonrefined high tensile steel having high strength and enabling an alloy saving by treating steel contg. a prescribed percentage each of C, Si and Mn as basic components while suitably combining the conditions of heating and rolling with those of accelerated cooling after the rolling. CONSTITUTION: Steel is prepared contg. 0.13W0.30% C, 0.25W0.60% Si and 0.50W2.20% Mn as basic components or further contg. ≥1 kind among Cu, Ni, Cr, etc. The steel is heated to the Ac 3 point or above and subjected to controlled rolling making the grains fine, especially rolling in a temp. zone under the recrystallization temp. to form unrecrystallized austenite grains. Before the unrecrystallized austenite recrystallizes, the steel is acceleratedly cooled at 1W60, especially 5W30°C/sec cooling rate without delay. Simultaneously with the accelerated cooling, dehydrogenation is effected by vacuum degassing or other method so as to control hydrogen Hc in the steel at the central part in the plate thickness direction to Hc(ppm) ≤1.10- 0.005σy. Thus, the desired nonrefined high tensile steel is manufactured. COPYRIGHT: (C)1981,JPO&Japio

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 0 · Forward citations: 12.

Claims (0)

No claim text indexed for this record.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (0)

No backward patent references recorded.