Abstract
PROBLEM TO BE SOLVED: To dissolve the deterioration of the reliability of a product and the increase in the cost at the time of flattening interlayer insulating films by stacking the interlayer insulating films of a first type which are flattened by a chemical mechanical polishing(CMP) method, and the interlayer insulating films of a second type which are flattened by a spin on glass film application method. SOLUTION: Interlayer insulating films 6 and 20 flattened by a CMP method and interlayer insulating films 13 and 27 flattened by an SOG film application method are alternately stacked on a semiconductor substrate 40. Whole time when the interlayer insulating films receive polishing stress can be reduced compared to a case when the interlayer insulating films flattened by the CMP method are stacked. Since plasma silicon oxide films 10, 12, 24 and 26 having the inner stress of an opposite direction are used in the interlayer insulating films 13 and 27 flattened by the SOG film application method, inner tension stress can be relaxed.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 0 · Forward citations: 9.
Claims (0)
No claim text indexed for this record.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (9 of 9 total)
References Cited — Backward Prior Art (0)
No backward patent references recorded.