Method for correcting defect of phase inversion mask
Abstract
PROBLEM TO BE SOLVED: To facilitate correction by forming a phase inversion layer thicker than the thickness at which phase inversion occurs and edging the phase inversion layer as it is in the event of the occurrence of a defect. SOLUTION: In case edging residues are produced in the phase inversion layer 22 of an inverted translucent region 27 or a defective region 28, such as the occurrence of damage in the phase inversion layer 22, arises, a second resist pattern 26 is removed and the phase inversion layer 22 of the translucent region 25 and the phase inversion layer 22 of the inverted translucent region 27 are simultaneously subjected to dry process edging. At this point, an edging stopper layer 21 is used for the end point of the edging. The defective region 28 formed in the phase inversion layer 22 of the inverted translucent region 27 is removed and simultaneously, the translucent region 25 is edged by allowing the phase inversion layer 22 to remain at a thickness (d). The phase inversion mask maintaining the thickness (d) of the phase inversion as it is from the adjacent patterns is eventually formed. Even if the defect arises in the phase inversion layer 22 of the transluc
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 0 · Forward citations: 2.
Claims (0)
No claim text indexed for this record.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (2 of 2 total)
References Cited — Backward Prior Art (0)
No backward patent references recorded.