Lithium titanate, its production and lithium battery using the same

26Forward Citations (#2782566 Global)
0.9/yrCitation Velocity (#7904488 Global)
7.36Citation PageRank (#1763476 Global)
0Prior Art Cited
0Structured Claims
0Drawings / Sheets

Abstract

PROBLEM TO BE SOLVED: To obtain lithium titanate having many voids and controlled in particle size and shape by heating and dehydrating lithium titanate hydrate obtained by reacting a titanic acid compound with a lithium compound in water. SOLUTION: A titanium compound is reacted with an ammonium compound in water at 0-50 deg.C to afford a titanic acid compound. The titanic acid compound is reacted with a lithium compound at >=50 deg.C, as necessary, in water containing 0.01-5mol/L ammonium compound to provide lithium titanate hydrate. The lithium titanate hydrate is dried at 30-200 deg.C and heated at 200-800 deg.C and dehydrated to provide the lithium titanate having a laminate structure, 1-300m<2> /g specific surface area and 0.1-50μm longest particle diameter and having voids in particles.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 0 · Forward citations: 26.

Claims (0)

No claim text indexed for this record.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (0)

No backward patent references recorded.