Optical recording material composed of antimony-tin alloy containing third element
Abstract
PURPOSE: To give the combination of a small crystallization speed, a favorable corrosion resistance, a stable amorphous state and a high speed and high density recording capability to an optical recording material by a method wherein another specific element is included in an alloy including specified amounts of and ratio of Sb and Sn. CONSTITUTION: The alloy of an once-write type amorphous thin film optical recording layer includes the amounts and ratio of Sb and Sn, in which the crystalline laser recorded mask of the alloy has NaCl type or a slightly distorted NaCl type crystals. Further, the alloy includes at least one other element excluding In, Al, Zn or Ge. The additional element in the alloy rises an amorphous to crystalline transition temperature. The rise of the amorphous to crystalline transition temperature is important for the long term stability of a recording substance. The recording layer having the higher transition temperature has a low automatic amorphous to crystalline transition temperature. In addition, when this recording substance is employed for an optical recording, an improved carrier-to-noise ratio is developed.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 4 · Forward citations: 8.
Claims (0)
No claim text indexed for this record.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗