Adherent material to be bonded and bonding
Abstract
PURPOSE:To obtain an adherent material to be bonded especially suitable for bonding of very small spots by setting a bondable resin layer on an electconductive substrate by electrophoresis. CONSTITUTION:A resin such as acrylic, epoxy, polyester, polyamide, polyurethane, PE or polyacrylic acid resin is diluted with desalted water into 1-50% solution to give an electrophoresis solution. A substrate is placed on an anode based on a counter electrode in the solution in the case of an anionic system and on a cathode in the case of a cationic system and applied voltage and time are controlled by using DC electric source to form a bonding layer having desired film thickness. An excellent bonding layer having 1-30mum thickness is usually formed at 20-200V applied voltage, 0.5-3A/dm<2> current density for 10-180 seconds treatment time. After washing with water, the material to be bonded is predried at about 50-60 deg.C for about 5 minutes, another material to be bonded is stuck to a given position of the material and redried at 80-200 deg.C by a furnace for about 10-30 minutes to bond both the materials completely.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 0 · Forward citations: 1.
Claims (0)
No claim text indexed for this record.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (1 of 1 total)
| Patent | Title | Year | Citations |
|---|---|---|---|
| US 6,588,095 B2 | Method of processing a device by electrophoresis coating | 2003 | 4 |
References Cited — Backward Prior Art (0)