Production of high toughness steel

1Forward Citations (#61776650 Global)
0.0/yrCitation Velocity (#59036558 Global)
0.74Citation PageRank (#61776650 Global)
2Prior Art Cited
0Structured Claims
0Drawings / Sheets

Abstract

PURPOSE:To produce a steel having excellent toughness at high productivity by starting rolling after holding the solidified steel to the specific temp. more than the lower limit temp., which is possible to recrystallize to austenitic structure, for the specific time, and completing the rolling having the specific rolling reduction ratio at more than the specific temp. after executing the specific rolling. CONSTITUTION:After casting and solidifying the molten steel, the steel is held at more than the lower limit temp., which is possible to recrystallize to the austenitic structure, and <=1300 deg.C for >=5min during being at >=Ar3 point temp. After that, the rolling is started at the temp. more than the lower limit temp., which is possible to recrystallize to the austenitic structure, and the rolling is executed at >=10% of casting thickness. The rolling of >=2 rolling reduction ratio containing this rolling is completed at >=Ar3 point temp. To the steel, 0.005-0.20wt.% C, 0.001-0.025% S, 0. 01-0.80% Si, <=0.1, Al, 0.20-2.00% Mn are contained. Further, Nb, Ti, Cu, Zr, etc., may be contained. By this method, the steel having excellent toughness can be produced at

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 2 · Forward citations: 1.

Claims (0)

No claim text indexed for this record.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (1 of 1 total)

PatentTitleYearCitations
US 8,316,558 B2Shoe20128