Manufacturing method of carbon interior ore
Abstract
PROBLEM TO BE SOLVED: To provide a manufacturing method of carbon interior ore capable of manufacturing agglomerated ore having high reduction reactivity and collapse strength, and good reduction powdering property.SOLUTION: After heating dehydrating a pellet obtained by granulating a mixture of a powdered iron ore containing crystal water and a hydraulic binder at 300 to 600°C, CVI treatment using crude COG at 500 to 1000°C as a raw material gas is conducted on the pellet at a state with heating at 300 to 600°C. A carbon material derived from gas-like tar contained the crude COG is precipitated and almost completely filled in pores generated in the powder iron ore by heating dehydration and thereby carbon interior ore having high reduction reactivity and collapse strength, and good reduction powdering property can be manufactured. The carbon interior ore can be manufactured at low cost because crude COG can be used as the raw material gas for the CVI treatment and the pellet can be CVI treated at relatively low temperature by using sensible heat of crude COG.SELECTED DRAWING: Figure 3
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 9 · Forward citations: 8.
Claims (0)
No claim text indexed for this record.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗