Release coating having low friction coefficient

1Forward Citations (#54218733 Global)
0.1/yrCitation Velocity (#49190690 Global)
0.81Citation PageRank (#54218733 Global)
0Prior Art Cited
0Structured Claims
0Drawings / Sheets

Abstract

PROBLEM TO BE SOLVED: To provide a release layer, which achieves both of a low friction coefficient and stable low releasing force and which does not exhibit decrease in adhesion strength, when used in a field of an adhesive tape, caused by transfer of some components in a release coating to the adhesive after being in contact with the tape.SOLUTION: A release coating composition is provided, essentially comprising a release agent and from 0.01 wt.% to 30 wt.% (on a basis of the whole composition) of a fine particulate additive in a form of three-dimensional bodies based on a polymer produced from vinyl structural units.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 0 · Forward citations: 1.

Claims (0)

No claim text indexed for this record.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (1 of 1 total)

References Cited — Backward Prior Art (0)

No backward patent references recorded.