Abstract

PROBLEM TO BE SOLVED: To provide a method for highly efficiently manufacturing a cold-rolled steel sheet excellent in deep drawability.SOLUTION: A steel ingot or a steel billet is prepared, which contains, by mass, <0.010% C, ≤1.5% Si, ≤2.0% Mn, ≤0.10% P, ≤0.010% S, 0.0005-0.10% Al, ≤0.0060% N, 0.001-0.10% Ti, 0.001-0.10% Nb, while satisfying a relation: (C/12+N/14+S/32)/(Ti/48+Nb/93)≤1.4, and the balance being Fe with impurities. The steel ingot or steel billet is subjected to: hot-rolling to be completed at a temperature of ≥(Arpoint-30°C); cooling to 750°C at an average cooling rate of ≥400°C/sec within a period of 0.5 seconds after completion of the hot-rolling; pickling after coiling at a temperature of ≥400°C and <640°C; cold-rolling with a rolling reduction of 60-95%; and annealing at a temperature of 750-880°C.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 10 · Forward citations: 1.

Claims (0)

No claim text indexed for this record.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (1 of 1 total)

PatentTitleYearCitations
JP 2016156079 AFerritic thin steel sheet—16