PROBLEM TO BE SOLVED: To provide an oriented magnetic steel plate with magnetic domain refinement by electron beam irradiation and which achieves excellent low-noise characteristics when assembled on an existing transformer.SOLUTION: In the oriented magnetic steel plate, the ratio (Wa/Wb) between a film thickness (Wa) of a fosterite coating on a distortion introduction side of the steel plate and a film thickness (Wb) of the fosterite coating on a distortion non-introduction side is 0.5 or greater; the average width of a discontinuous section in a magnetic domain in the steel plate surface on the distortion introduction side is 150-300 [mu]m; and the average width of the discontinuous section in the magnetic domain in the steel plate surface on the distortion non-introduction side is 250-500 [mu]m.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 8 · Forward citations: 29.
Claims (0)
No claim text indexed for this record.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗