Aluminum alloy plate to be formed, and manufacturing method therefor
Abstract
<P>PROBLEM TO BE SOLVED: To inexpensively provide an aluminum alloy plate to be formed, which has adequate hem-bending formability, low bending anisotropy and further superior baking hardenability after coating, causes little aging at room temperature, and has adequate ridging mark resistance. <P>SOLUTION: The aluminum alloy plate is made of an Al-Mg-Si-based alloy or an Al-Mg-Si-Cu-based alloy; satisfies each condition of (C<SB>1/10</SB>+C<SB>1/4</SB>)/2 > C<SB>1/2</SB>and 30 < (C<SB>1/10</SB>+C<SB>1/4</SB>) < 500, when C<SB>1/10</SB>, C<SB>1/4</SB>and C<SB>1/2</SB>are defined as cube orientation density at respective positions of 1/10, 1/4 and 1/2 deep from the sheet surface in a sheet thickness direction; has ä001}<210> orientation density in a range of 2 to 50, in a 1/10 to 1/4 deep region in the sheet thickness direction; and has 0 degree and 90 degrees earing rates of 5% or higher. The manufacturing method includes strictly prescribed casting and hot rolling conditions. The conditions for metallographic structures in a cast slab and a plate after having b
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 19 · Forward citations: 32.
Claims (0)
No claim text indexed for this record.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗