Polypropylenic resin pre-expanded particle and in-mold expansion molded product
Abstract
<P>PROBLEM TO BE SOLVED: To provide an in-mold expansion molded product which is made by a commonly used molding machine satisfying withstand pressure specifications of 0.4 MPa, and which has surface beautifulness and high rigidity. <P>SOLUTION: In a polypropylenic resin pre-expanded particle, the resin having an MFR of 5-20 g/10 min and a melting point of 140°C-155°C, and satisfying the conditional formula; [MFR(g/10 min)]≥1.6×[melting point (°C)]-235 is used as a base resin. The in-mold expansion molded product is made by molding the pre-expanded particle. <P>COPYRIGHT: (C)2006,JPO&NCIPI
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 8 · Forward citations: 21.
Claims (0)
No claim text indexed for this record.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗