Copper alloy powder for build up excellent in cladding performance and wear resistance, and valve seat using the same
Abstract
<P>PROBLEM TO BE SOLVED: To provide copper alloy powder for build up by laser, the powder excellent in cladding performance, wear resistance and finishing workability, and also to provide a valve seat using the same. <P>SOLUTION: The copper alloy powder for build up contains, by mass %, 7-20% Ni, ≤10% Fe+Co, 2-5% Si, 0.01-0.1% C, 0.1-10% in total of at least one or more of Al, Zn, Sn, Mn, Cr, Ti and Zr, and the balance Cu and inevitable impurities. Also, this copper alloy powder satisfies an equation of 3Ni+5(Fe+Co)+7Si≤100 and is excellent in cladding performance and wear resistance. In addition to the above components, it further contains ≤5% Mo, ≤2% B, ≤2% P, and ≤4% V. The invention includes a valve seat using this copper alloy powder for build up. <P>COPYRIGHT: (C)2006,JPO&NCIPI
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 0 · Forward citations: 15.
Claims (0)
No claim text indexed for this record.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗