Lamination ceramic electronic component and paste for lamination ceramic electronic component
Abstract
<P>PROBLEM TO BE SOLVED: To provide a lamination ceramic electronic component which can reduce a generation of delamination. <P>SOLUTION: A ceramic layer 20 is mainly formed by ceramic dielectric material having a first ceramic particle 31. An auxiliary layer 30 is mainly formed by ceramic dielectric material having a second ceramic particle 32, and a plane in which an inner electrode 12 is formed, furthermore buries a portion in which the inner electrode does not exist. When a mean particle diameter of the first ceramic particle 31 is set to be α (μm), and a weight of a particle which is 1.043×α (μm) or more and 1.122×α (μm) or less in diameter is set to be A, furthermore a weight of a particle which is 0.886×α (μm) or more and 0.965×α (μm) or less in diameter is set to be B, a ratio A/(A+B) satisfies 0.30≤A/(A+B)≤0.65. <P>COPYRIGHT: (C)2006,JPO&NCIPI
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 0 · Forward citations: 9.
Claims (0)
No claim text indexed for this record.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (9 of 9 total)
References Cited — Backward Prior Art (0)
No backward patent references recorded.