Method of manufacturing fluidization treated material
Abstract
<P>PROBLEM TO BE SOLVED: To provide a fluidization treated material of stable quality. <P>SOLUTION: Sand of 75 μm to 2 mm in grain size is filtered from slurry obtained by adding and mixing water in construction removed soil, and silt of 10-75 μm in grain size is separated by centrifugal separation of the remaining slurry to extract clay of 10 μm or less in grain size. The sand, silt and clay, or silt and clay are mixed at a predetermined ratio, and a water-setting material and water are further added to form slurry, thus providing the fluidization treated material. <P>COPYRIGHT: (C)2006,JPO&NCIPI
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 0 · Forward citations: 1.
Claims (0)
No claim text indexed for this record.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (1 of 1 total)
| Patent | Title | Year | Citations |
|---|---|---|---|
| JP 2007247324 A | Manufacturing method for lightweight soil | — | 1 |
References Cited — Backward Prior Art (0)
No backward patent references recorded.