Patents
JP 2005290521 A#6710163 Most CitedExpiredJapan (JPO)Utility

Copper alloy foil provided with roughening-treated face and roughening treatment method for copper alloy foil

14Forward Citations (#6710163 Global)
0.7/yrCitation Velocity (#11247743 Global)
3.43Citation PageRank (#6103272 Global)
0Prior Art Cited
0Structured Claims
0Drawings / Sheets

Abstract

<P>PROBLEM TO BE SOLVED: To provide roughening-treated rolled copper alloy foil in which craters as the remarkable defect characteristic of rolled copper alloy foil provided with a roughening-treated face are reduced, further to provide rolled copper alloy foil having high strength, adhesive strength with a resin layer, acid resistance, tinning liquid resistance and high peel strength, further provided with satisfactory etching properties and glossiness and suitable for a flexible printed circuit board capable of the fine-patterning of wiring, and to provide a roughening treatment method therefor. <P>SOLUTION: The copper alloy foil provided with a roughening-treated face is characterized in that the number of craters present in the roughening-treated face of the rolled copper alloy foil subjected to roughening treatment with copper fine particles is ≤10 pieces/25 mm<SP>2</SP>. The roughening treatment method for copper alloy foil is characterized in that roughening plating is performed under the conditions that: the content of copper sulfate is 3 to 50 g/L expressed in terms of Cu; the content of nickel sulfate is 1 to 50 g/L expressed in terms of Ni; the co

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 0 · Forward citations: 14.

Claims (0)

No claim text indexed for this record.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (14 of 14 total)

PatentTitleYearCitations
JP 7,356,209 B2表面処理銅箔、樹脂層付き表面処理銅箔、キャリア付銅箔、積層体、プリント配線板の製造方法及び電子機器の製造方法20230
US 8,449,987 B2Rolled copper or copper alloy foil with roughened surface and method of roughening rolled copper or copper alloy foil20136
JP 2015026654 ACopper foil with carrier, and copper clad laminate using the same—10
CN 104,946,924 AStrong-wear-resisting material—1
US 9,049,795 B2Rolled copper or copper-alloy foil provided with roughened surface20150
US 2009162685 A1Rolled Copper or Copper Alloy Foil with Roughened Surface and Method of Roughening Rolled Copper or Copper Alloy Foil—27
JP 2018172785 ASurface-treated copper foil, surface-treated copper foil with resin layer, copper foil with carrier, laminate, method for producing printed wiring board and method for producing electronic apparatus—25
CN 102,061,494 BThe roughened method of process Copper Foil and untreated Copper Foil and copper clad panel20160
CN 102,061,494 AProcessed copper foil, coarsening treatment method of unprocessed copper foil and laminated plate with copper foil applied—6
JP 2011105960 ATreated copper foil, method for roughening untreated copper foil, and copper-clad laminate—5
JP 2011040727 AAdhesive film with copper foil—24
JP 2017193778 ACopper foil, copper foil for high frequency circuit, copper foil with carrier, copper foil with carrier for high frequency circuit, laminate, method for manufacturing printed wiring board and method for producing electronic apparatus—7
US 8,252,166 B2Method of roughening rolled copper or copper alloy foil20125
JP 2011040728 ACopper clad laminate—27

References Cited — Backward Prior Art (0)

No backward patent references recorded.