Abstract
<P>PROBLEM TO BE SOLVED: To provide a method for manufacturing a copper red glass by which stable copper red is developed in mass production scale by paying attention to the oxidation/reduction atmosphere of a base glass and the content of iron and adding various kinds of metals and the oxides to stabilize the color development of copper and copper oxide being coloring components. <P>SOLUTION: In the method for manufacturing the colored glass by adding a colorant to the base glass fused in a fusing furnace in a colorant forehearth, the base glass is constituted so that the existing ratio formed between Fe<SP>2+</SP>and Fe<SP>3+</SP>in the glass satisfies Fe<SP>2+</SP>/(Fe<SP>2+</SP>Fe<SP>3+</SP>)≥0.4 and the content of iron in the glass is 0.01-0.5 wt.% expressed in terms of ferric oxide. The colorant is a flit or a pellet prepared by blending one or both of copper and copper oxide as the coloring components with one or more kinds of metals such as tin, selenium, cobalt, chromium, nickel or manganese or the metallic oxides. <P>COPYRIGHT: (C)2004,JPO
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 0 · Forward citations: 11.
Claims (0)
No claim text indexed for this record.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (11 of 11 total)
References Cited — Backward Prior Art (0)
No backward patent references recorded.