Wire with flux for gas shield arc welding
Abstract
PROBLEM TO BE SOLVED: To provide a wire with flux for a gas shield arc welding which improves the strength and the toughness of a welded metal and has a high sticking performance, a productivity, a low generation of slag and a deep penetration performance of a solid wire, and at the same time an excellent weld workability of a wire with flux. SOLUTION: The wire for an arc welding is filled with a steel outer skin flux, the wire in total includes, in mass %, 0.05 to 1.8% arc stabilizing agent, 0.02 to 0.15% C, 0.02 to 1.8% Si, 0.8 to 4.0% Mn, >1.5 to 3.0% Ni, 0.05 to 0.7% Mo, 0.02 to 3.0% Ti, and further, if necessary, <=0.01% B, and the degree of filling flux is 3 to 10%. The filled arc stabilizing agent included by as much as 1.8% or less in the wire is a synthesized material which includes one or two of Na2 O and TiO2 , consisting of <=0.6% Na2 O expressed in terms of Na2 O and <=1.8% TiO2 expressed in terms of TiO2 .
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 0 · Forward citations: 5.
Claims (0)
No claim text indexed for this record.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (5 of 5 total)
References Cited — Backward Prior Art (0)
No backward patent references recorded.