PROBLEM TO BE SOLVED: To provide a cellulose acrylate film with such advantages that the stability over time of a liquid after dissolution is improved and the optical characteristics, mechanical strength and dimensional stability after manufacturing the film are outstanding. SOLUTION: The cellulose acrylate film is manufacturing through the step to dissolve a cellulose acrylate in a substantially non-chlorine solvent and prepare a cellulose acrylate solution, the step to manufacture the cellulose acrylate film using the cellulose acrylate solution and the step to stretch the film. Thus the obtained film shows that the Re retardation value is within the range of 20 to 115 nm, the Rth retardation value is within the range of 70 to 400 nm and the in-plane average absolute value of a retarded phase axial angel is 3 deg. or less and the standard deviation of the retarded phase axial angle is 1.5 deg. or less.

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 11 · Forward citations: 22.

Claims (0)

No claim text indexed for this record.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

Cited By — Indexed Forward Citations (15 of 22 total)