Polycarbonate resin/abs resin extrusion board
Abstract
PROBLEM TO BE SOLVED: To provide a PC(polycarbonate) resin excellent in vacuum formability and pneumatic formability and an extrusion board composed of an ABS resin as a main component. SOLUTION: The extrusion board is formed by extruding a resin composition mainly composed of the PC resin of 30-70 pts.wt. and the ABS resin of 70-30 pts.wt. (sum total is 100 pts.wt.). The coefficient of storage elasticity of the extrusion board with a frequency of 1 Hz is 1.00×106 Pa or more at 170 deg.C and 2.00×105 Pa or more at 200 deg.C both in the flow direction and in the direction which intersects perpendicularly with the flow direction when forming when measured by a tensile strength method using a dynamic viscoelasticity spectrometer. A composition whose weight average molecular weight is 106-5×106 and has a linear structure and composed of a copolymer of a methacrylic ester and an acrylic ester or a copolymer composed of different kinds of methacrylic esters as fundamental constitution components is added to the above resin composition in the range of 1-10 pts.wt. to the total of 100 pts.wt. of the PC resin and the ABS resin.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 0 · Forward citations: 6.
Claims (0)
No claim text indexed for this record.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (6 of 6 total)
References Cited — Backward Prior Art (0)
No backward patent references recorded.