Fe-Ni ALLOY POWDER AND ITS MANUFACTURE

4Forward Citations (#22550654 Global)
0.1/yrCitation Velocity (#38241898 Global)
4.28Citation PageRank (#4272972 Global)
0Prior Art Cited
0Structured Claims
0Drawings / Sheets

Abstract

PROBLEM TO BE SOLVED: To provide an Fe-Ni soft magnetic alloy powder improved in magnetic properties to a greater extent and reduced in core loss at a low cost. SOLUTION: This alloy powder has a composition consisting of, by weight, 35-85% Ni, 1.0-4.5% Si, <=0.15% Mn, and the balance Fe with impurities, satisfying >20 Si/Mn, and containing, if necessary, <=5.5% Al and <=5.5% Mo. The alloy powder is composed of a water atomized powder and has a grain size properly coarsened in such a way that the value of d/D50 exceeds 0.10 (where d is the average value of grain diameter and D50 is average particle diameter).

Interactive Citation Constellation Global Citation Ranking

Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 0 · Forward citations: 4.

Claims (0)

No claim text indexed for this record.

Technical Overview & Description

Full multi-page specification text is archived at the issuing office. Read complete official specification ↗

References Cited — Backward Prior Art (0)

No backward patent references recorded.