Cemented carbide and its production
Abstract
PROBLEM TO BE SOLVED: To provide a hard material based on submicron WC in a bonding phase having hardenability. SOLUTION: In cemented carbide in which a bonding phase having hardenability is incorporated with 50 to 90 mass % submicron WC, the bonding phase is composed of Fe, 10 to 60 mass % Co, <10 mass % Ni, 0.2 to 0.8 mass % C and Cr, W and optional Mo and/or V by the quantity satisfying the following relational inequality of 2xC<xW+xCr+xMo+xV<2.5xC, where (x) denotes the molar fractional ratio of the elements in the bonding phase, and the total Cr content satisfies the following relational inequality of 0.03<Cr (mass %)/(100-WC (mass %))<0.05. Moreover, the bonding phase is composed of martensite having the fine dispersion of, preferably, M2C type lattice-matched carbides having the size of 10 nm order by several %.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 0 · Forward citations: 12.
Claims (0)
No claim text indexed for this record.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (12 of 12 total)
References Cited — Backward Prior Art (0)
No backward patent references recorded.