Manufacture of secondary power supply
Abstract
PROBLEM TO BE SOLVED: To allow rapid charge/discharge, and improve voltage resistance, capacity, energy density, and cycle reliability, by impregnating an element where a positive electrode is faced to a negative electrode through a separator into an electrolyte, and then charging the element at a specific current density, and storing lithium ions in a carbon material. SOLUTION: A current density when lithium ions are stored in a negative electrode carbon material is 0.01-100 A per 1 g carbon material. Once the lithium ions are stored, the current density is not required to be adjusted during subsequent charge/discharge. Thickness of a negative electrode is 7-70% of thickness of a positive electrode. The thickness of the positive electrode is preferably 80-250 μm. In the carbon material, surface interval of the [002] surface due to X-ray diffraction is preferably 0.335-0.410 nm. Especially, graphite based carbon material is preferable. A solvent of the electrolyte preferably contains at least 70 wt.% propylene carbonate.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 0 · Forward citations: 3.
Claims (0)
No claim text indexed for this record.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (3 of 3 total)
References Cited — Backward Prior Art (0)
No backward patent references recorded.