Glass base board for information recording medium and its manufacture; magnetic recording medium using such base board and its manufacture
Abstract
PROBLEM TO BE SOLVED: To enable high-density recording and reproduction while maintaining stable and excellent characteristic by setting roughness on the main surface of a glass base board at a specific value or less. SOLUTION: The roughness on the main surface of a glass base board is set at Rmax<=15 nm, Ra<=1 nm, and Rq<=1.5 nm. Rq is a root-mean-square root(RMS). The glass base board made of alumino-silicate glass cut out in a shape of a disk is ground with a diamond stone, and is further ground by brushing so that the surface roughness on the end face is approximately 1 μm at Rmax and 0.3 μm at Ra. After sandblast, lapping with alumina abrasive grain, and No.1 to No.3 grinding with abrasive powder, chemical strengthening is performed and then the glass base board 1 is obtained. Formed successively on the base board 1 are the first substrate 2, second substrate 3, ruggedness formed layer 4, third substrate 5, magnetic layer 6, protective layer 7 and a lubricant layer 8. The intrasurface distribution in the magnetic recording medium and the variance of the magnetic recording medium within a pallet are suppressed, and the stability is thereby improved.
Interactive Citation Constellation Global Citation Ranking
Interactive SVG Citation Constellation renders in Rust/WebAssembly. Prior art cited: 0 · Forward citations: 6.
Claims (0)
No claim text indexed for this record.
Technical Overview & Description
Full multi-page specification text is archived at the issuing office. Read complete official specification ↗
Cited By — Indexed Forward Citations (6 of 6 total)
References Cited — Backward Prior Art (0)
No backward patent references recorded.